Add to polyester gelcoat resin at a ratio of 2 to 5% of the gelcoat volume when the gelcoat is required to cure exposed to air. This prevents the gelcoat curing with a 'tacky' surface.
Do not use when the gelcoat is in a mould & is going to be overlaid by a laminate.